????atural materials A and B, which are grinded into powder, are to be mixed evenly. Natural material B will be disclosed by request. ???The mixed materials are put into molding. Heat and pressure is applied. Pressure:40 kg/cm2 ???In 5 to 10 minutes stiff hard board can be obtained.